Symptom: Swelling
Possible Causes: What could cause this problem?
Surface contamination
Sample Testing: How do you measure?
1.
Extract contamination into solvent
2.
Dry onto ATR crystal or IR window
3.
Measure using transmission
Data Analysis Plan: How do you identify the problem?
1.
Search libraries to identify contamination
2.
Determine if polymer or formulation is appropriate for application
Recommended Configuration: What to use?
Nicolet iS5 FT-IR spectrometer
iD7 Diamond ATR accessory
OMNIC Specta software for Polymer Labs
Resources: Learn More
Nicolet iS5 FT-IR brochure
Nicolet iS5 FT-IR video
How to Use the ATR Technique video
Polymer Analysis Kits for FT-IR Guide
FT-IR Contaminant Identification using OMNIC Specta Software application note
Enhanced Sensitivity to Detect Phthalates by FT-IR application note